Description
Large rounded air bubbles or blisters, usually occurring in the area of seams and boxed in corners, or over heavily filled plastic surfaces.
Cause
Air trapped beneath the paint expands, resulting in the detachment of the paint film from the substrate. This frequently results from:
Prevention
Rectification
The paint must be removed to the depth of the bubble, any underlying defect remedied and the area repainted.